Titanium alloy can not only make marine equipment develop towards "deep, large, far, high ", but also fully realize the same life as the main body of marine equipment. It is the best choice for marine equipment. At present, China pays more attention to the application of titanium in marine equipment, and the amount of titanium used is also increasing. Deep-sea pressure shell, seawater pipeline, cylinder superstructure, frame, etc. will become the key development direction of marine titanium.

Actualment, hi ha moltes aplicacions de titani a la indústria naviliera a casa ia l'estranger.
However, the material system in relevant specifications is not perfect. It is hoped that relevant units will organize discussion and improve the material system in current relevant codes such as Titanium Pressure Vessel, Material and Welding, so as to facilitate the designer's reference.
Upper buildings:
Actualment, hi ha alguns exemples d'aplicació en la superestructura de vaixells de guerra domèstics, com ara Ti70 (TA23) per al pal, la barra TA5 i TA7 per a l'antena de radar, la placa TA2 i TA5 per a la pell de l'hangar i l'estructura del marc.
El titani també s'utilitza àmpliament a les zones superiors de l'edifici del vaixell de transport del moll amfibi LPD17, reduint la seva massa al voltant d'un 50 per cent i millorant considerablement la seva estabilitat.
Aplicacions de producció en altres àrees
A més de la gran quantitat de titani que s'utilitza a la carcassa resistent a la pressió-anterior, el sistema de canonades i la superestructura, altres components també són útils en equips marins a casa i a l'estranger.